An inspector sees a patch of metal through the dark exterior of an Epson MC-306. The supplier says the unit has a metal case under the mold compound. The inspector wonders whether the body has been damaged. Start with the full order number and place the sample beside its applicable drawing. Epson’s specific Q13MC30620006xx document says that the metal case can show at the top or bottom and describes that condition as cosmetic. Apply that note to matching observations. Record any additional body crack, shifted terminal, dent, or scratch on its own before making a disposition.
Compare the exposed area with the applicable drawing
Photograph the top, side, and bottom. Identify the lot, orientation, and magnification. First establish whether the metal is visible on a surface described by Epson. Then inspect the adjacent compound for a fracture crossing the edge, lifting, or missing material. For a new reel, retain an unassembled comparison specimen and check agreed positions along the reel. The acceptance record can refer to the exact drawing and previously approved sample images. Ask the supplier’s technical team to review a location or appearance outside that description, using the agreed sampling procedure. The note supplies no universal area threshold that converts every exposure into an acceptable part.
The specific sheet uses the final two characters to identify the quantity and packing arrangement. Keep the complete number from Q13MC30620006xx and verify what the supplied suffix represents. A label abbreviated to MC-306 and frequency calls for a mapping to the original manufacturer number and its specification. Different loads in the family can look the same and oscillate in the same test fixture. Establish part, load, and lot before classifying the exposure. Keep separate check fields for the appearance evidence and the identity evidence. That permits a clear visual decision while material with an unresolved identity remains out of use.
Lighting can make photos of one specimen look like two different problems. Retain the originals and add a scale, one diffuse-light image, and one oblique-light image. The metal can reflect differently with angle. Examine a possible crack at several focal planes for a continuous edge. Mark any indentation in the image and keep the sample as received before cleaning or scraping it. Tie dimensions and electrical results to the same specimen. If the supplier replies with a photo of another normal unit, ask the technical reviewer to say whether the allowance covers the observed form and document the basis for the incoming instruction.
Check assembled clearance independently of cosmetic acceptance
The applicable drawing prohibits external connections to pins 2 and 3. Check the package view and board. Their proximity to metal does not make them a shield return. If the part sits near a battery spring or conductive cover, include the exposed region and nearby conductive parts in the assembly review. Epson’s cosmetic note addresses the component itself, whereas the project must prevent contact in its own design. For example, the drawing’s maximum part height is 2.54 mm. Suppose the minimum board-to-cover distance is 2.64 mm. Simple subtraction leaves 0.10 mm. With another 0.04 mm for solder lift and 0.03 mm for board deflection, only 0.03 mm remains. Recalculate for the actual mechanical stack.
At first article, fit the cover in the approved worst-case assembly position and retain open, closed, and normal loading observations. If the clock stops only with the cover installed, document the repeatable symptom. With power off, inspect for unintended contact, then use the same fixture to compare specimens with and without visible metal. Record where the spring or fixture contacted the board before changing its position. A clock that resumes when the cover is removed calls for an assembly investigation. If individual specimens still fail under valid electrical conditions, send the images, lot, and test conditions to the manufacturer for review. This keeps a mechanical interaction traceable to the affected board.
Use the correct load to verify frequency
For Q13MC30620006xx, Epson specifies a 6 pF load, ±20 ppm initial room-temperature tolerance, and 50 kΩ maximum motional resistance. Multiplying 32,768 Hz by 20 parts per million gives 0.65536 Hz. The initial window is 32,767.34464 to 32,768.65536 Hz. A valid fixture reading of 32,768.35 Hz is high by 0.35 Hz, or about 10.68 ppm, and is within that initial window. Measure motional resistance separately. A passing frequency gives no value for it. If the incoming fixture is still configured for 12.5 pF from an earlier part, establish the correct load and use actual measurement uncertainty for a result near the limit.
Put the drawing’s visual allowance in the incoming instruction and define which observations require a sample hold or engineering test. The record can separately identify top or bottom exposure, any additional damage, manufacturer code, electrical results, and interference observed in assembly. A 32.768 kHz passive crystal that meets the applicable visual and electrical criteria can proceed when the project has approved the enclosure clearance. If that first article is pending, the purchase agreement may permit basic material acceptance while release to production remains at engineering trial. Component appearance and assembled performance then each have evidence that can be reviewed for a new supplier or enclosure.