A compact industrial wireless board previously ran in a dry enclosure. It will now be potted for moisture protection. The board uses the same NDK NX1612SA crystal, frequency and assembly. Engineering wants to test only the finished sample, and purchasing plans to reuse the existing specification. NDK gives special instructions for resin molding and asks users to discuss the exact delivery specification and evaluation procedure. Useful evidence includes paired measurements of the same 40 MHz crystal on the same board before and after the process, with an unpotted control that sees equivalent time and heat.
Check the component limits and the board process
NDK data sheet NDKX03-00035-001 identifies NX1612SA with STD-CIS-4 and includes 40.000 MHz in the frequency table. The applicable configuration is fundamental mode with 8 pF load and 60 Ω maximum ESR. At 40 MHz, the initial tolerance at 25°C is ±10 ppm. Temperature characteristics relative to +25°C are ±12 ppm. The specified operating range is −30°C to +85°C. Match these to the complete order and actual document revision. The precautions say molding resin can affect characteristics and ask customers to work through the delivery specification and evaluation method and assess samples. A component-level pass and a completed board after a customer process need their own evidence.
Describe the requested process to the manufacturer. Include resin, coverage, whether it crosses the metal lid, cure time and temperature, and assembly sequence. If the design leaves an uncovered region around the crystal, mark it on the board drawing. Obtain documentation applicable to the proposed process, and build first articles under the real cure sequence. A different resin or cure may need a fresh review. The qualification record should identify exactly what was used on each board and which conditions the supplier confirmed.
Record paired changes and compare them with the control
At 40 MHz, 1 ppm is 40 Hz. Suppose a board is at 40,000,160 Hz before potting and 39,999,880 Hz after the process at the same controlled temperature. It moves by −280 Hz, or −7 ppm. Suppose an unpotted control exposed to equivalent heat and elapsed time moves from 40,000,080 to 40,000,040 Hz, a difference of −40 Hz or −1 ppm. Subtracting the changes gives an estimated process difference of −240 Hz or −6 ppm. These hypothetical values do not isolate a material mechanism. Resin stress, moisture and changes in parasitics can all affect the outcome.
The final potted-board reading in the example is 120 Hz low, or −3 ppm relative to nominal. It may still meet the complete clock's room-temperature requirement. If the project separately allocates ±5 ppm, or ±200 Hz, to potting, the estimated −240 Hz process change exceeds that allowance by 40 Hz. The process and final function can therefore yield different decisions. Recheck temperature, reference, load and settling before enlarging the trial. One stabilized room-temperature comparison does not establish start-up or frequency over the full temperature range.
Keep the manufacturer acknowledgment with the process record
Complete incoming checks on loose parts and assemble boards from the same lot. Record the board, crystal lot and load capacitors. Use a buffered measurement point where possible so probing does not change the two crystal terminals' load. Define cooling and waiting time and reuse the same equipment to observe frequency and repeated cold and hot starts. An unpotted control with the same heat exposure can improve identification of the process difference. Preserve the fixture and measurement point because residual heat, fixture movement and changed cables can affect a comparison.
Distinguish a shift measured soon after cure from a shift measured after a defined wait. During the first test, the resin and the area around the crystal may not yet be at the same temperature used for comparison. Define cooling criteria for the first reading and a fixed later point for retest. For aging or humidity work, record the time origin and room-temperature recovery. Several paired points can distinguish a one-time process shift from drift during subsequent use.
State whether measurements are made in the enclosure. An unpotted control should otherwise follow the same process sequence. If only the potted group is screwed into the housing, mounting pressure is another variable. First match the mounting, then run an additional controlled enclosure comparison. If a supplier later changes the lid or base material, repeat the paired evaluation on an approved board with the same resin and process.
When evaluating another resin, run it with the approved board version. If slow start or frequency shift appears only with resin, compare coverage, cure sequence and temperature before expanding to other lots. If the unpotted control shifts along with the potted board, check heat exposure, circuit and instrument first. Put the actual material, process, manufacturer response and test bounds in the release record for the potted board. Use a sample order while the individual delivery conditions are open, and release after the paired board results and manufacturer evidence are both applicable.