A stored OX-228 still oscillates. How should its terminal solderability be retested?

A warehouse finds a reel of oven-controlled oscillators bought early in the project. Every tested unit produces a clock and the terminals look normal, but several boards on the new line show poor joints at final inspection. Frequency measurements cannot establish whether the terminals will solder well. To transfer the reel, request the lot’s terminal finish and solderability conditions, then use controlled samples to distinguish component terminals, board surfaces and the assembly process.

The data sheet has separate reflow and solderability requirements

Page 5 of the Microchip OX-228 data sheet gives a recommended reflow profile and a separate solderability entry. The latter lists dip-and-look testing, eight hours of damp pretreatment and more than 95% wetting, with conditions dependent on termination type. For an actual order, match the package option and data sheet revision and establish whether a result is type qualification, periodic sampling or a test of this reel. Passing a reflow profile trial alone does not establish that the reel’s terminals still have the required coverage after storage and handling.

Epson’s crystal handling precautions also note that prolonged unsuitable temperature or humidity can affect frequency stability or solderability. A date code supports traceability. Check the package, terminal plating, original bag, storage history, opening and repacking. If a reel contains mixed date codes or finish lots, several good-looking samples cannot represent all of it. Moisture exposure on the line is handled according to the actual device rating. Terminal solderability needs evidence of the actual surface and soldering process. A compliant moisture-removal bake does not establish that oxidation or contamination has gone.

Coverage measures what stayed. A wetting curve also shows when it started.

For dip-and-look, use the specified method to identify the area that must wet. Suppose one evaluated terminal has 1.00 mm² of area and 0.92 mm² is wetted, giving 92% coverage. If the applicable contract criterion is greater than 95%, record that terminal as nonconforming. A second terminal with 0.99 mm² of coverage would bring the two-terminal average to 95.5%. The average can hide the first defect. Apply the agreed terminal-level or sampling rule. Follow the test conditions for whether edges, cut surfaces or excluded areas count. Orient and label the inspected surfaces in photographs so another reviewer can check them.

For comparing how two lots wet, the public description of IEC 60068-2-69 explains force-based wetting balance measurements. They record force over time after contact with the solder. Check the method and decision rule specified in the contract. One force trace has no universal pass line. An IPC wetting-balance method gives the simplified net force relationship F = Pγ cos θ − B, where P is contact perimeter, γ is surface tension and B represents buoyancy. Equal forces can indicate different conditions when sample perimeter or immersion differs.

For two illustrative witness terminals with the same shape, assume perimeter 2.0 mm, surface tension 0.50 N/m and buoyancy 0.30 mN. A net force of 0.50 mN gives a corrected surface-tension term of 0.80 mN, or 80% of the ideal model maximum of 1.0 mN. Another group with net force 0.10 mN gives 40% after correction. This example shows how to compare like conditions. Real terminal surfaces are complex, so use the actual wetting time, alloy and flux conditions. An assumed surface tension is not a measured material property. Interpret visual results using continuous coverage and defect location as well.

Both lots can pass final dip coverage while behaving differently in the first few seconds. For example, one lot reaches an agreed force in 1.2 s and the other in 2.6 s in the same fixture and process, with similar final forces. If production has a short effective solder contact window, the slower lot needs assessment under representative assembly conditions. Solder-bath contact time cannot be transferred directly to time above liquidus in a reflow oven. Heating, flux activity and contact area differ. Use the same time origin, curve point and buoyancy correction to compare wetting speed.

For borderline visual coverage, have two inspectors review images using the same view and lighting. A shadow that changes the identified area by 0.03 mm² produces a three-percentage-point difference on a 1.00 mm² terminal. Retain original images and area annotations if reviewers disagree, and use a more reproducible agreed method if needed. Sample positions across trays or tape and record exposed terminal orientation to detect surface changes limited to one part of the packaging.

Run a line trial that can locate the cause

  1. Sample the lot randomly and retain untreated controls. Choose the test according to the agreed termination type, alloy, flux, pretreatment and sample plan. Keep dip and wetting-balance samples identified separately from units for assembly.
  2. Alternate known solderable controls with suspect stock at comparable pad locations on representative boards. Hold stencil, solder paste, board finish and oven run constant. Record failure locations by pad and terminal. If both groups fail, check the board and process first. If the difference follows the stored lot, ask the supplier to verify its finish and storage evidence.
  3. Keep joint evidence alongside electrical results. An intermittent signal can temporarily recover under contact pressure. A subsequent pass cannot supersede evidence of a poor joint. If necessary, have quality engineering arrange cross-sectioning or other failure analysis, retaining photographs and same-reel sample identities.

Archive the complete order code, lot, storage condition, planned process, sampling basis, photographs and failure disposition. If the storage history is missing, an approved test of the actual stock may supply further evidence. If the supplier proposes replating or retinning, establish responsibility, package risks, changes to marking and which electrical and solderability checks must be repeated. A transfer decision then applies to the identified lot and assembly process with supporting evidence beyond an earlier power-on check.

WeChat

MERLIN · TIMING COMPONENTS

Scan with WeChat to contact Sales

Add our WeCom contacts from your usual WeChat app.

On desktop, scan with your phone. On mobile, save the QR image and select it from your album in WeChat Scan.